Описание
Отзывы
Описание

GB/T 19466.3 – 2009/ISO 11357-3:1999 Part 6 Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) during oxidation induction period;
GB/T 19466.2 – 2004/ISO 11357-2:1999 Part 2: Determination of glass transition temperature;
GB/T 19466.3 – 2004/ISO 11357-3:1999 Part 3: Determination of melting and crystallization temperature and enthalpy.
GB/T 19466.4 – 2016/ISO 11357-4:1999 Part 4: Determination of specific heat capacity;
The DSC-300 series is a high-precision differential scanning calorimeter. The sensor is made of imported E-couple, with high sensitivity. The signal acquisition circuit is shielded and protected, with strong anti-interference and high baseline stability.
Touch screen operation can be used for glass transition temperature test, phase transition test, melting and enthalpy value test, product stability test and oxidation induction period test. Wide application range
Features
1. Industrial-level 7-inch touch screen displays rich information.
2. New metal furnace body structure, better baseline and higher accuracy. The heating adopts indirect conduction mode, with high uniformity and stability, and reduces pulse radiation, which is superior to the traditional heating mode.
3. USB communication interface has strong versatility, reliable and uninterrupted communication, and supports self-recovery connection function.
4. Automatic switching of two-way air flow, fast switching speed and short stabilization time. At the same time, add a protective gas input.
5. The software is simple and easy to operate.
Specifications
1. Temperature range: – 170 ℃~600 ℃ liquid nitrogen refrigeration
2. Temperature resolution: 0.001 ℃
3. Temperature fluctuation: ± 0.01 ℃
4. Temperature repeatability: ± 0.01 ℃
5. Heating rate: 0.1~100 ℃/min/0.1~40 ℃/min
6. Constant temperature time: program setting ≤ 24h
7. Temperature control mode: temperature rise, constant temperature, temperature drop (fully automatic program control)
8. DSC range: 0 ~ ± 600mW
9. DSC resolution: 0.01uW
10. DSC accuracy: 0.01mW
11. Working power supply: AC220V/50Hz or customized
12. Atmosphere control gas: nitrogen, oxygen (automatic instrument switching)
13. Gas flow: 0-300mL/min
14. Gas pressure: ≤ 5MPa
15. Display mode: 24bit color, 7-inch LCD touch screen display
16. Data interface: standard USB interface
17. Parameter standard: equipped with reference materials (indium, tin), users can calibrate the temperature by themselves
18. The upper computer is a three-in-one operation software, which is also suitable for the combination of thermogravimetric and synchronous instruments.
19. The instrument has multiple sets of thermocouples, one set of test sample temperature, one set of test furnace temperature, and one set of test instrument internal ambient temperature
20. Cooling device: liquid nitrogen refrigeration.